Brící teasfhulangacha inslithe is príomhábhair riachtanacha iad sa réimse tionsclaíochta ardteochta. Bíonn tionchar dírea...
LÉIGH TUILLEADH
Alumina Hollow Ball Cáblaí HG-165 | Alumina Hollow Ball Cáblaí HG-160 | Muilite Ard-neart Castables Éadrom HG-145 | Mullite Ard-neart Castables Éadrom HG-140 | Mullite Éadrom Castables HG-135 | Mullite Éadrom Castables HG-130 | ||
Teocht Oibriúcháin ℃ | 1650 | 1600 | 1450 | 1400 | 1350 | 1300 | |
Bulcdlúis(g/cm³) | 1.5 | 1.5 | 1.7 | 1.7 | 1.4 | 1.4 | |
Neart Comhbhrú (Mpa) | 110 ℃ × 24 uair an chloig | 7.5 | 17 | 25 | 25 | 6 | 5.5 |
1300 ℃ × 3 h | 20 | 22 | 20 | 20 | 5 | 5 | |
Athruithe Tar éis Dó Sreang % ℃×3h | 0. 4(1600) | 0. 5(1500) | 0. 6(1450) | 0. 8(1400) | 0. 7(1350) | 0. 7(1300) | |
Seoltacht Theirmeach (w/m.k) | 400 ℃ | 0.42 | 0.42 | 0.58 | 0.58 | 0.40 | 0.38 |
800 ℃ | 0.48 | 0.48 | 0.64 | 0.64 | 0.45 | 0.43 | |
Comhpháirteanna Ceimiceacha | Al2O3 ≥ | 98 | 94 | 70 | 68 | 65 | 65 |
Fe2O3 ≤ | 0.3 | 0.3 | 0.8 | 0.9 | 0.9 | 1.0 |
Castables Éadrom Inslithe Teasa agus Teirmeacha | ||||||||
HG-130 | HG-125 | HG-120 | HG-110 | HG-100 | HG-90 | HG-80 | ||
Teocht Oibriúcháin ℃ | 1300 | 1250 | 1200 | 1100 | 1000 | 900 | 800 | |
Bulcdlúis (g/cm³) | 1.4 | 1.3 | 1.2 | 1.1 | 1.0 | 0.8 | 0.6 | |
Neart Comhbhrúite 1000 ℃ × 3h Mpa | 5 | 6 | 4 | 4 | 4 | 1.7 (900 ℃ × 3h) | 0.6 (800 ℃ × 3h) | |
Athruithe Tar éis Dó Sreang % ℃×3h | 0.6 (1300) | 0.7 (1250) | 0.6 (1200) | 0.6 (1100) | 0.5 (1000) | 0.7 (900) | 0.5 (800) | |
Seoltacht Theirmeach 600 ℃ w/m.k | 0.36 | 0.33 | 0.32 | 0.30 | 0.28 | 0.25 | 0.17 | |
Comhpháirteanna Ceimiceacha % | AL2O3 ≥ | 43 | 42 | 38 | 32 | 30 | 28 | 28 |
Nascáil Cré Plaisteacht | Ard-Teocht teasfhulangach Plaisteacht | Mullite Plaisteacht Dóiteáin | Corundum teasfhulangacha Plaisteacht | Cairbíd Sileacain Plaisteacht Dóiteáin | ||
Bulcdlúis (g/cm³) | 2.35 | 2.60 | 2.60 | 3.00 | 2.60 | |
Friotaíocht Dóiteáin ℃ > | 1700 | 1720 | 1750 | 1790 | 1790 | |
Neart Comhbhrú (Mpa) | 110 ℃ × 24 uair an chloig | 15 | 40 | 42 | 45 | 45 |
600 ℃ × 3 h | 20 | 60 | 65 | 65 | 68 | |
1300 ℃ × 3 h | 35 | 70 | 75 | 80 | 80 | |
Aththéigh Athrú Líneach % ℃ × 3h | ±0.2 (1400) | ±0.3 (1400) | ±0.3 (1450) | ±0.3 (1500) | ±0.3 (1400) | |
Cobhsaíocht Turraing Teirmeach /Amanna | 30 | 30 | 30 | 30 | 30 | |
Comhpháirteanna Ceimiceacha | Al2O3 ≥ | 55 | 72 | 73 | 92 | - |
Fe2O3 % ≤ | 1.2 | 1.1 | 0.8 | 0.3 | - | |
SiO2 ≥ | - | - | - | - | 71 |
Brící teasfhulangacha inslithe is príomhábhair riachtanacha iad sa réimse tionsclaíochta ardteochta. Bíonn tionchar dírea...
LÉIGH TUILLEADHBrící teasfhulangacha inslithe ról ríthábhachtach a bheith acu sa réimse tionsclaíoch ardteochta, agus bíonn tionchar dír...
LÉIGH TUILLEADHBrící teasfhulangacha inslithe ról ríthábhachtach a bheith acu sa réimse tionsclaíoch ardteochta, agus tá a bpróiseas mún...
LÉIGH TUILLEADHBrící teasfhulangacha inslithe Is ábhar ríthábhachtach iad ar féidir leo cobhsaíocht struchtúrach agus feidhmíocht inslit...
LÉIGH TUILLEADHRefractories monolithic ról tábhachtach a bheith acu i dtrealamh tionsclaíoch ardteochta, agus tá tionchar díreach ag a d...
LÉIGH TUILLEADH